Refractory firebricks with thermal insulation have a porous structure and excellent thermal insulation properties, resulting in low thermal conductivity and superior insulation. This allows for a decrease in lining thickness during shaft operation and a quick rise in operating temperature with less fuel, resulting in cost savings and improved productivity as well as energy savings.

Item\Product A type
A-1 A-2 A-3 A-4 A-5 A-6 A-7
Temp(℃) Reheating Shrinkage Less than 2.0% 900 1000 1100 1200 1300 1400 1500
Bulk density 0.50 0.50 0.50 0.55 0.60 0.70 0.75
Cold Crushing Strength(N/㎟) 0.49 0.50 0.50 0.55 0.60 0.70 0.75
Thermal Conductivity (kcal/mh℃) at 350℃ 0.13 0.14 0.15 0.16 0.17 0.20 0.22
Applicable Usage The external and internal lining of various furnaces
Item\Product B type
B-1 B-2 B-3 B-4 B-5 B-6 B-7
Temp(℃) Reheating Shrinkage Less than 2.0% 900 1000 1100 1200 1300 1400 1500
Bulk density 0.70 0.70 0.75 0.80 0.80 0.90 1.00
Cold Crushing Strength(N/㎟) 2.46 2.46 2.46 2.46 2.46 2.95 2.95
Thermal Conductivity (kcal/mh℃) at 350℃ 0.17 0.18 0.20 0.22 0.23 0.27 0.31
Applicable Usage The external and internal lining of various furnaces
Item\Product C type
C-1 C-3 C-5
Temp(℃) Reheating Shrinkage Less than 2.0% 1300 1400 1500
Bulk density 1.10 1.20 1.25
Cold Crushing Strength(N/㎟) 4.91 6.87 9.81
Thermal Conductivity (kcal/mh℃) at 350℃ 0.30 0.38 0.45
Applicable Usage The external and internal lining of various furnaces
Item\Product S type
S-1 S-3 S-5
Temp(℃) Reheating Shrinkage Less than 2.0% 1300 1400 1500
Bulk density 1.4 1.45 1.5
Cold Crushing Strength(N/㎟) 14.71 14.71 14.71
Thermal Conductivity (kcal/mh℃) at 350℃ 0.50 0.55 0.60
Applicable Usage The external and internal lining of various furnaces